FXBW-04 Acrylic Acid Modified Polysiloxane Finish _PAINTS & COVERING_PRODUCTS_TAIHANG

FXBW-04 Acrylic Acid Modified Polysiloxane Finish

1960978680891da.png

FXBW-04 Acrylic Acid Modified Polysiloxane Finish (different colors) (use for steel structures)

Characteristics: excellent elements resistance、resistance of ultraviolet radiation irradiation property、excellent resistance of acid、alkali、oil、water and antifouling property、good gloss and color retention and high gloss decorative (gloss and color retention is the acrylic acid polyurethane paint more than 4 times)、innoxious、environmental protection.

Uses: mainly use for bridge、stadiums、conference and exhibition center、airport、petrochemical plant etc. steel structure anticorrosion.

Technical target
Mixing ratio: Host crystal/Firming agent=100/8(by weight)
Standard film thickness: Dry: 30μm/coat
Academic spreading rate: 0.07kg/ ㎡/30μm
Solid contents: 70%
Humidity requirement: below 85%
Drying time & Coating interval

Temperature (℃)

10

02

30

Dry to touch(hrs)

60

50

25

Dry semi-hard(hrs)

12

8

6

Min. interval(hrs)

24

12

8

Substrate treatmentPrimer surface must thoroughly clean、dry、no dew

Matching
Applicable under coatings: Epoxy primers、epoxy intermediate paint

Contact with us now